ER316LSI

Class: ER316LSI

AWS: A5.9

Conforms to Certification: AWS A5.9                  ASME SFA A5.9

Weld Process Used for Tig (GTAW)

AWS Chemical Composition Requirements
C = 0.03 max
Cr = 18.0 – 20.0
Ni = 11.0 – 14.0
Mo = 2.0 – 3.0
Mn = 1.0 – 2.5
Si = 0.65 – 1.00
P = 0.03 max
S = 0.03 max
Cu = 0.75 max

Available Sizes
.030 x 36
.035 x 36
.045 x 36
1/16 x 36
3/32 x 36
1/8 x 36
3/16 x 36
5/32 x 36

Application
ER316LSI affords the same characteristics as 316L. The high silicon allows better arc stability along with minimal post-weld grinding. The low carbon in the weld metal gives excellent assurance against intergranular corrosion.

Deposited Chemical Composition % (Typical)
C = 0.02 Mo = 2.50 P = 0.010
Cr = 18.50 Mn = 1.70 S = 0.013
Ni = 11.50 Si = 0.90

 

Mechanical Properties (R.T.) 
Yield Strength 58,000psi
Tensile Strength 88,000psi
Elongation 37%
Reduction of Area 68%

Deposited All Weld Metal Properties
Data is typical for ER316LSI weld metal deposited by Tig using 100% Argon as the shielding gas.

Recommended Welding Parameters
GTAW “Tig Process”
Wire Diameter Amps DCSP Volts Shielding Gas
.035 60-90 12-15 Argon 100%
.045 80-110 13-16 Argon 100%
1/16 90-130 14-16 Argon 100%
3/32 120-175 15-20 Argon 100%

Note: Parameters for tig welding are dependent upon plate thickness and welding position.